Products
PRODUCTS DETAILS
Home > Products >
CuNi2 NC005 2.0802 Cupronickel Wire Perfect Solution For Stress Corrosion Cracking And Pitting Resistance

CuNi2 NC005 2.0802 Cupronickel Wire Perfect Solution For Stress Corrosion Cracking And Pitting Resistance

MOQ: 5kg
Standard Packaging: Packed with waterproof paper or weave bag, into pallets or wooden case. Special packaging requirements can also be accommodated.
Delivery Period: 3 days
Payment Method: T/T, D/P
Supply Capacity: 30 Tons per day
Detail Information
Place of Origin
China
Brand Name
Senphus
Certification
ISO9001
Model Number
CuNi2/NC005/2.0802/C70260
Place Of Origin:
Jiangsu, China
Type:
Nickel Wire
Application:
Heating,household Electrical Application
Color:
Silvery White/bright Or Oxidized
Product Name:
CuNi2 NC005 Copper Nickel Wire
Resistivity:
0.05 ±10%
Melting Temperature In ℃:
1090
Density At 20℃ (g/cm³):
8.9
Min.tensile Strength In N/mm²:
220
Elongation:
25
Highlight:

CuNi2 cupronickel wire

,

NC005 cupronickel wire

,

Perfect copper nickel alloy wire

Product Description

CuNi2 NC005 2.0802 Cupronickel Wire Perfect Solution For Stress Corrosion Cracking And Pitting Resistance

 

CuNi2, a copper-nickel alloy containing approximately 2% nickel, is a versatile material known for its combination of good corrosion resistance, moderate mechanical strength, and excellent thermal and electrical conductivity. This alloy is particularly suited for applications requiring durability, ease of fabrication, and stable performance under various environmental conditions.

 

With a composition of 98% copper and 2% nickel, CuNi2 retains most of copper's desirable properties while benefiting from the addition of nickel. The nickel content improves its resistance to oxidation and corrosion, particularly in moist or mildly aggressive environments.

 

GB ISO ASTM DIN/EN JIS GOST AS

CuNi2

NC005

CuNi2Si C70260

CuNi2

2.0802

C70260

C7026

C70260

MH2

702B

C70260

 

Main physical properties:

Max continuous operating temperature ℃ 200
Resistance temperature coefficient x 10-5/℃(20℃-600℃) <120
Thermovoltage to copper at 20℃ in  μV/K -12
Thermal expansion coefficient ×10-6/K(20℃-400℃) 17.5
Thermal conductance at 20℃ W/mK 130
Specific heat capacity at 20℃ J/gK 0.38

 

 

 

 

 

 

 

 

 

 

 

 

Some key features of CuNi2 include:

  • Good Corrosion Resistance:

Provides enhanced resistance to tarnishing and corrosion compared to pure copper, making it suitable for mildly corrosive environments.

  • High Thermal and Electrical Conductivity:

Maintains excellent conductivity for heat and electricity, making it ideal for applications such as electrical wiring and heat exchangers.

  • Ductility and Workability:

Highly malleable and easy to fabricate, allowing for production in various forms like wires, sheets, and rods.

  • Improved Strength:

Slightly stronger than pure copper while retaining good flexibility and toughness.

  • Aesthetic Appearance:

Offers a pleasing reddish appearance, often used in decorative or architectural applications.

 

 

Applications:

  • Electrical Industry:

Used in connectors, conductors, and cables, where high electrical conductivity and corrosion resistance are essential.

  • Heat Exchangers and Cooling Systems:

Ideal for thermal applications due to its high thermal conductivity and ability to withstand moderate environmental conditions.

  • Coinage and Tokens:

Commonly used in minting coins and tokens for its aesthetic appeal, corrosion resistance, and machinability.

  • Decorative Applications:

Found in architectural elements, ornamental pieces, and jewelry, where its color and resistance to tarnish are valued.

  • Automotive and Aerospace Components:

Utilized in components like radiators, fuel lines, and hydraulic systems, where conductivity and corrosion resistance are beneficial.

  • Marine Applications:

Occasionally used in non-critical marine components due to its ability to resist mild seawater corrosion.

 

Conclusion

CuNi2 is a durable and efficient material that offers a balance between the properties of pure copper and the enhanced corrosion resistance of nickel. Its excellent conductivity, workability, and corrosion resistance make it an ideal choice for a variety of industrial, electrical, and decorative applications, ensuring reliable performance and longevity in diverse environments.

 

 

Main technical data

Type CuNi1 NC003 CuNi2 NC005 CuNi4 NC007 CuNi6 NC010 CuNi8 NC012 CuMn3 NC012 CuNi10 NC015 CuNi14 NC020 CuNi19 NC025 CuNi23 NC030 CuNi30 NC035 CuNi34 NC040 CuNi44 NC050
Composition(%) Cu Rest Rest Rest Rest Rest Rest Rest Rest Rest Rest Rest Rest Rest
Mn / / / / / 3 / 0.3 0.5 0.5 1.0 1.0 1.0
Ni 1 2 4 6 8   10 14.2 19 23 30 34 44
Max.continuous operating temperature(℃) 200 200 200 220 250 200 250 300 300 300 350 350 400
Resistivity at 20℃(μ m) 0.03
±10%
0.05
±10%
0.07
±10%
0.10
±10%
0.12
±10%
0.12
±10%
0.15
±10%
0.20
±5%
0.25
±5%
0.30
±5%
0.35
±5%
0.40
±5%
0.49
±5%
Resisitance-temperature coefficient 20-600℃ (×10-5/℃) < 100 < 120 < 50 < 60 < 57 < 38 < 50 < 38 < 25 < 16 < 10 < -0 < -6
Thermovoltage to
copper at 20℃ in (μV/K)
-8 -12 -12 -18 -22 1 -25 -28 -32 -34 -37 -39 -43
Mean coefficient of linear thermal expansion, in (10-6/K) , at a temperature between 20 ℃ and 400 ℃ 17.5 17.5 17.5 17.5 17.5 18 17.5 17.5 17.5 17.5 17.0 16.0 15.0
Thermal conductance
at 20℃ (W/mK)
145 130 130 92 75 84 59 48 38 33 27 25 23
Specific heat capacity at 20℃ in (20℃ J/gK) 0.38 0.38 0.38 0.38 0.38 0.39 0.38 0.38 0.38 0.38 0.39 0.40 0.41
Density at 20 ℃(g/cm3) 8.9 8.9 8.9 8.9 8.9 8.8 8.9 8.9 8.9 8.9 8.9 8.9 8.9
Melting temperature in (℃) 1085 1090 1090 1095 1097 1050 1100 1115 1135 1150 1170 1180 1280
Min.tensile strength in (N/mm2) 210 220 220 250 270 290 290 310 340 350 400 400 420
Elongation(%) 25 25 25 25 25 25 25 25 25 25 25 25 25

 

 

Technical data table

Diameter(mm) NC003 CuNi1 NC005 CuNi2 NC007 CuNi4 NC010 CuNi6 NC012 CuNi8 NC015 CuNi10 NC020 CuNi14 NC025 CuNi19 NC030 CuNi23 NC035 CuNi30 NC040 CuNi34 NC050 CuNi44
0.10 3.82 6.36 8.91 12.73 15.28 19.09 25.46 31.83 38.19 44.56 50.93 62.39
0.11 3.16 5.26 7.37 10.52 12.63 15.78 21.04 26.30 31.56 36.82 42.09 51.56
0.12 2.65 4.42 6.19 8.84 10.61 13.26 17.68 22.10 26.52 30.94 35.37 43.33
0.13 2.26 3.76 5.27 7.53 9.04 11.30 15.07 18.83 22.60 26.36 30.14 36.92
0.14 1.95 3.24 4.55 6.49 7.80 9.74 12.99 16.24 19.48 22.73 25.98 31.83
0.15 1.70 2.82 3.96 5.65 6.79 8.48 11.31 14.14 16.97 19.80 22.64 27.73
0.16 1.49 2.48 3.48 4.97 5.97 7.46 9.95 12.43 14.92 17.40 19.89 24.37
0.17 1.32 2.20 3.08 4.40 5.29 6.60 8.81 11.01 13.21 15.41 17.62 21.59
0.18 1.18 1.96 2.75 3.92 4.72 5.89 7.86 9.82 11.78 13.75 15.72 19.26
0.19 1.06 1.76 2.47 3.52 4.23 5.29 7.05 8.81 10.58 12.34 14.11 17.28
0.20 0.95 1.59 2.23 3.18 3.82 4.77 6.36 7.95 9.54 11.14 12.73 15.60
0.21 0.87 1.44 2.02 2.88 3.46 4.33 5.77 7.21 8.66 10.10 11.55 14.15
0.22 0.79 1.31 1.84 2.63 3.16 3.94 5.26 6.57 7.89 9.20 10.52 12.89
0.23 0.72 1.20 1.68 2.40 2.89 3.61 4.81 6.01 7.22 8.42 9.63 11.79
0.24 0.66 1.10 1.55 2.21 2.65 3.31 4.42 5.52 6.63 7.73 8.84 10.83
0.25 0.61 1.01 1.43 2.03 2.44 3.05 4.07 5.09 6.11 7.13 8.15 9.98
0.26 0.57 0.94 1.32 1.88 2.26 2.82 3.77 4.70 5.65 6.59 7.53 9.23
0.27 0.52 0.87 1.22 1.74 2.10 2.61 3.49 4.36 5.23 6.11 6.99 8.56
0.28 0.49 0.81 1.14 1.62 1.95 2.43 3.25 4.06 4.87 5.68 6.50 7.96
0.29 0.45 0.75 1.06 1.51 1.82 2.27 3.03 3.78 4.54 5.29 6.06 7.42
0.30 0.42 0.70 0.99 1.41 1.70 2.12 2.83 3.53 4.24 4.95 5.66 6.93
0.31 0.40 0.66 0.93 1.32 1.59 1.98 2.65 3.31 3.97 4.63 5.30 6.49
0.32 0.37 0.62 0.87 1.24 1.49 1.86 2.49 3.11 3.73 4.35 4.97 6.09
0.33 0.35 0.58 0.82 1.17 1.40 1.75 2.34 2.92 3.51 4.09 4.68 5.73
0.34 0.33 0.55 0.77 1.10 1.32 1.65 2.20 2.75 3.30 3.85 4.41 5.40
0.35 0.31 0.51 0.73 1.03 1.25 1.55 2.08 2.60 3.11 3.63 4.16 5.09
0.36 0.29 0.49 0.69 0.98 1.18 1.47 1.96 2.46 2.94 3.43 3.93 4.81
0.37 0.28 0.46 0.65 0.93 1.12 1.39 1.86 2.33 2.79 3.25 3.72 4.56
0.38 0.26 0.44 0.62 0.88 1.06 1.32 1.76 2.20 2.64 3.08 3.53 4.32
0.40 0.24 0.39 0.56 0.79 0.95 1.19 1.59 1.99 2.38 2.78 3.18 3.90
0.41 0.23 0.37 0.53 0.76 0.91 1.13 1.51 1.89 2.27 2.65 3.03 3.71
0.42 0.22 0.36 0.51 0.72 0.87 1.08 1.44 1.80 2.16 2.52 2.89 3.54
0.43 0.21 0.34 0.48 0.69 0.83 1.03 1.38 1.72 2.06 2.41 2.75 3.37
0.44 0.20 0.32 0.46 0.66 0.79 0.98 1.31 1.64 1.97 2.30 2.63 3.22
0.45 0.19 0.31 0.44 0.63 0.75 0.94 1.26 1.57 1.88 2.20 2.52 3.08
0.46 0.18 0.30 0.42 0.60 0.72 0.90 1.20 1.50 1.80 2.10 2.41 2.95
0.47 0.17 0.28 0.40 0.58 0.69 0.86 1.15 1.44 1.72 2.01 2.31 2.82
0.48 0.17 0.27 0.39 0.55 0.66 0.82 1.10 1.38 1.65 1.93 2.21 2.71
0.49 0.16 0.26 0.37 0.53 0.64 0.79 1.06 1.33 1.59 1.85 2.12 2.60
0.50 0.15 0.25 0.36 0.51 0.61 0.76 1.01 1.27 1.52 1.78 2.04 2.50
0.51 0.15 0.24 0.34 0.49 0.59 0.73 0.98 1.22 1.46 1.71 1.96 2.40
0.52 0.14 0.23 0.33 0.47 0.57 0.70 0.94 1.18 1.41 1.65 1.88 2.31
0.53 0.14 0.22 0.32 0.45 0.54 0.67 0.91 1.13 1.35 1.59 1.81 2.22
0.54 0.13 0.22 0.31 0.44 0.52 0.65 0.87 1.09 1.30 1.53 1.75 2.14
0.55 0.13 0.21 0.29 0.42 0.51 0.63 0.84 1.05 1.26 1.47 1.68 2.06
0.56 0.12 0.20 0.28 0.41 0.49 0.60 0.81 1.02 1.21 1.42 1.62 1.99
0.57 0.12 0.19 0.27 0.39 0.47 0.58 0.78 0.98 1.17 1.37 1.57 1.92
0.58 0.11 0.19 0.27 0.38 0.45 0.56 0.76 0.95 1.13 1.32 1.51 1.85
0.59 0.11 0.18 0.26 0.37 0.44 0.54 0.73 0.91 1.09 1.28 1.46 1.79
0.60 0.11 0.18 0.25 0.35 0.42 0.53 0.71 0.88 1.06 1.24 1.41 1.73
  • Tolerance of ohm/m: ±5%
  • Round wire: range from 0.04mm (0.0016″) to 12mm (0.4724″)
  • Ribbon: range from 0.05mm (0.002″) to 6mm (0.2362″), Max ratio width : thickness = 10:1

CuNi2 NC005 2.0802 Cupronickel Wire Perfect Solution For Stress Corrosion Cracking And Pitting ResistanceCuNi2 NC005 2.0802 Cupronickel Wire Perfect Solution For Stress Corrosion Cracking And Pitting ResistanceCuNi2 NC005 2.0802 Cupronickel Wire Perfect Solution For Stress Corrosion Cracking And Pitting Resistance

 

 

 

 

 

 

Products
PRODUCTS DETAILS
CuNi2 NC005 2.0802 Cupronickel Wire Perfect Solution For Stress Corrosion Cracking And Pitting Resistance
MOQ: 5kg
Standard Packaging: Packed with waterproof paper or weave bag, into pallets or wooden case. Special packaging requirements can also be accommodated.
Delivery Period: 3 days
Payment Method: T/T, D/P
Supply Capacity: 30 Tons per day
Detail Information
Place of Origin
China
Brand Name
Senphus
Certification
ISO9001
Model Number
CuNi2/NC005/2.0802/C70260
Place Of Origin:
Jiangsu, China
Type:
Nickel Wire
Application:
Heating,household Electrical Application
Color:
Silvery White/bright Or Oxidized
Product Name:
CuNi2 NC005 Copper Nickel Wire
Resistivity:
0.05 ±10%
Melting Temperature In ℃:
1090
Density At 20℃ (g/cm³):
8.9
Min.tensile Strength In N/mm²:
220
Elongation:
25
Minimum Order Quantity:
5kg
Packaging Details:
Packed with waterproof paper or weave bag, into pallets or wooden case. Special packaging requirements can also be accommodated.
Delivery Time:
3 days
Payment Terms:
T/T, D/P
Supply Ability:
30 Tons per day
Highlight

CuNi2 cupronickel wire

,

NC005 cupronickel wire

,

Perfect copper nickel alloy wire

Product Description

CuNi2 NC005 2.0802 Cupronickel Wire Perfect Solution For Stress Corrosion Cracking And Pitting Resistance

 

CuNi2, a copper-nickel alloy containing approximately 2% nickel, is a versatile material known for its combination of good corrosion resistance, moderate mechanical strength, and excellent thermal and electrical conductivity. This alloy is particularly suited for applications requiring durability, ease of fabrication, and stable performance under various environmental conditions.

 

With a composition of 98% copper and 2% nickel, CuNi2 retains most of copper's desirable properties while benefiting from the addition of nickel. The nickel content improves its resistance to oxidation and corrosion, particularly in moist or mildly aggressive environments.

 

GB ISO ASTM DIN/EN JIS GOST AS

CuNi2

NC005

CuNi2Si C70260

CuNi2

2.0802

C70260

C7026

C70260

MH2

702B

C70260

 

Main physical properties:

Max continuous operating temperature ℃ 200
Resistance temperature coefficient x 10-5/℃(20℃-600℃) <120
Thermovoltage to copper at 20℃ in  μV/K -12
Thermal expansion coefficient ×10-6/K(20℃-400℃) 17.5
Thermal conductance at 20℃ W/mK 130
Specific heat capacity at 20℃ J/gK 0.38

 

 

 

 

 

 

 

 

 

 

 

 

Some key features of CuNi2 include:

  • Good Corrosion Resistance:

Provides enhanced resistance to tarnishing and corrosion compared to pure copper, making it suitable for mildly corrosive environments.

  • High Thermal and Electrical Conductivity:

Maintains excellent conductivity for heat and electricity, making it ideal for applications such as electrical wiring and heat exchangers.

  • Ductility and Workability:

Highly malleable and easy to fabricate, allowing for production in various forms like wires, sheets, and rods.

  • Improved Strength:

Slightly stronger than pure copper while retaining good flexibility and toughness.

  • Aesthetic Appearance:

Offers a pleasing reddish appearance, often used in decorative or architectural applications.

 

 

Applications:

  • Electrical Industry:

Used in connectors, conductors, and cables, where high electrical conductivity and corrosion resistance are essential.

  • Heat Exchangers and Cooling Systems:

Ideal for thermal applications due to its high thermal conductivity and ability to withstand moderate environmental conditions.

  • Coinage and Tokens:

Commonly used in minting coins and tokens for its aesthetic appeal, corrosion resistance, and machinability.

  • Decorative Applications:

Found in architectural elements, ornamental pieces, and jewelry, where its color and resistance to tarnish are valued.

  • Automotive and Aerospace Components:

Utilized in components like radiators, fuel lines, and hydraulic systems, where conductivity and corrosion resistance are beneficial.

  • Marine Applications:

Occasionally used in non-critical marine components due to its ability to resist mild seawater corrosion.

 

Conclusion

CuNi2 is a durable and efficient material that offers a balance between the properties of pure copper and the enhanced corrosion resistance of nickel. Its excellent conductivity, workability, and corrosion resistance make it an ideal choice for a variety of industrial, electrical, and decorative applications, ensuring reliable performance and longevity in diverse environments.

 

 

Main technical data

Type CuNi1 NC003 CuNi2 NC005 CuNi4 NC007 CuNi6 NC010 CuNi8 NC012 CuMn3 NC012 CuNi10 NC015 CuNi14 NC020 CuNi19 NC025 CuNi23 NC030 CuNi30 NC035 CuNi34 NC040 CuNi44 NC050
Composition(%) Cu Rest Rest Rest Rest Rest Rest Rest Rest Rest Rest Rest Rest Rest
Mn / / / / / 3 / 0.3 0.5 0.5 1.0 1.0 1.0
Ni 1 2 4 6 8   10 14.2 19 23 30 34 44
Max.continuous operating temperature(℃) 200 200 200 220 250 200 250 300 300 300 350 350 400
Resistivity at 20℃(μ m) 0.03
±10%
0.05
±10%
0.07
±10%
0.10
±10%
0.12
±10%
0.12
±10%
0.15
±10%
0.20
±5%
0.25
±5%
0.30
±5%
0.35
±5%
0.40
±5%
0.49
±5%
Resisitance-temperature coefficient 20-600℃ (×10-5/℃) < 100 < 120 < 50 < 60 < 57 < 38 < 50 < 38 < 25 < 16 < 10 < -0 < -6
Thermovoltage to
copper at 20℃ in (μV/K)
-8 -12 -12 -18 -22 1 -25 -28 -32 -34 -37 -39 -43
Mean coefficient of linear thermal expansion, in (10-6/K) , at a temperature between 20 ℃ and 400 ℃ 17.5 17.5 17.5 17.5 17.5 18 17.5 17.5 17.5 17.5 17.0 16.0 15.0
Thermal conductance
at 20℃ (W/mK)
145 130 130 92 75 84 59 48 38 33 27 25 23
Specific heat capacity at 20℃ in (20℃ J/gK) 0.38 0.38 0.38 0.38 0.38 0.39 0.38 0.38 0.38 0.38 0.39 0.40 0.41
Density at 20 ℃(g/cm3) 8.9 8.9 8.9 8.9 8.9 8.8 8.9 8.9 8.9 8.9 8.9 8.9 8.9
Melting temperature in (℃) 1085 1090 1090 1095 1097 1050 1100 1115 1135 1150 1170 1180 1280
Min.tensile strength in (N/mm2) 210 220 220 250 270 290 290 310 340 350 400 400 420
Elongation(%) 25 25 25 25 25 25 25 25 25 25 25 25 25

 

 

Technical data table

Diameter(mm) NC003 CuNi1 NC005 CuNi2 NC007 CuNi4 NC010 CuNi6 NC012 CuNi8 NC015 CuNi10 NC020 CuNi14 NC025 CuNi19 NC030 CuNi23 NC035 CuNi30 NC040 CuNi34 NC050 CuNi44
0.10 3.82 6.36 8.91 12.73 15.28 19.09 25.46 31.83 38.19 44.56 50.93 62.39
0.11 3.16 5.26 7.37 10.52 12.63 15.78 21.04 26.30 31.56 36.82 42.09 51.56
0.12 2.65 4.42 6.19 8.84 10.61 13.26 17.68 22.10 26.52 30.94 35.37 43.33
0.13 2.26 3.76 5.27 7.53 9.04 11.30 15.07 18.83 22.60 26.36 30.14 36.92
0.14 1.95 3.24 4.55 6.49 7.80 9.74 12.99 16.24 19.48 22.73 25.98 31.83
0.15 1.70 2.82 3.96 5.65 6.79 8.48 11.31 14.14 16.97 19.80 22.64 27.73
0.16 1.49 2.48 3.48 4.97 5.97 7.46 9.95 12.43 14.92 17.40 19.89 24.37
0.17 1.32 2.20 3.08 4.40 5.29 6.60 8.81 11.01 13.21 15.41 17.62 21.59
0.18 1.18 1.96 2.75 3.92 4.72 5.89 7.86 9.82 11.78 13.75 15.72 19.26
0.19 1.06 1.76 2.47 3.52 4.23 5.29 7.05 8.81 10.58 12.34 14.11 17.28
0.20 0.95 1.59 2.23 3.18 3.82 4.77 6.36 7.95 9.54 11.14 12.73 15.60
0.21 0.87 1.44 2.02 2.88 3.46 4.33 5.77 7.21 8.66 10.10 11.55 14.15
0.22 0.79 1.31 1.84 2.63 3.16 3.94 5.26 6.57 7.89 9.20 10.52 12.89
0.23 0.72 1.20 1.68 2.40 2.89 3.61 4.81 6.01 7.22 8.42 9.63 11.79
0.24 0.66 1.10 1.55 2.21 2.65 3.31 4.42 5.52 6.63 7.73 8.84 10.83
0.25 0.61 1.01 1.43 2.03 2.44 3.05 4.07 5.09 6.11 7.13 8.15 9.98
0.26 0.57 0.94 1.32 1.88 2.26 2.82 3.77 4.70 5.65 6.59 7.53 9.23
0.27 0.52 0.87 1.22 1.74 2.10 2.61 3.49 4.36 5.23 6.11 6.99 8.56
0.28 0.49 0.81 1.14 1.62 1.95 2.43 3.25 4.06 4.87 5.68 6.50 7.96
0.29 0.45 0.75 1.06 1.51 1.82 2.27 3.03 3.78 4.54 5.29 6.06 7.42
0.30 0.42 0.70 0.99 1.41 1.70 2.12 2.83 3.53 4.24 4.95 5.66 6.93
0.31 0.40 0.66 0.93 1.32 1.59 1.98 2.65 3.31 3.97 4.63 5.30 6.49
0.32 0.37 0.62 0.87 1.24 1.49 1.86 2.49 3.11 3.73 4.35 4.97 6.09
0.33 0.35 0.58 0.82 1.17 1.40 1.75 2.34 2.92 3.51 4.09 4.68 5.73
0.34 0.33 0.55 0.77 1.10 1.32 1.65 2.20 2.75 3.30 3.85 4.41 5.40
0.35 0.31 0.51 0.73 1.03 1.25 1.55 2.08 2.60 3.11 3.63 4.16 5.09
0.36 0.29 0.49 0.69 0.98 1.18 1.47 1.96 2.46 2.94 3.43 3.93 4.81
0.37 0.28 0.46 0.65 0.93 1.12 1.39 1.86 2.33 2.79 3.25 3.72 4.56
0.38 0.26 0.44 0.62 0.88 1.06 1.32 1.76 2.20 2.64 3.08 3.53 4.32
0.40 0.24 0.39 0.56 0.79 0.95 1.19 1.59 1.99 2.38 2.78 3.18 3.90
0.41 0.23 0.37 0.53 0.76 0.91 1.13 1.51 1.89 2.27 2.65 3.03 3.71
0.42 0.22 0.36 0.51 0.72 0.87 1.08 1.44 1.80 2.16 2.52 2.89 3.54
0.43 0.21 0.34 0.48 0.69 0.83 1.03 1.38 1.72 2.06 2.41 2.75 3.37
0.44 0.20 0.32 0.46 0.66 0.79 0.98 1.31 1.64 1.97 2.30 2.63 3.22
0.45 0.19 0.31 0.44 0.63 0.75 0.94 1.26 1.57 1.88 2.20 2.52 3.08
0.46 0.18 0.30 0.42 0.60 0.72 0.90 1.20 1.50 1.80 2.10 2.41 2.95
0.47 0.17 0.28 0.40 0.58 0.69 0.86 1.15 1.44 1.72 2.01 2.31 2.82
0.48 0.17 0.27 0.39 0.55 0.66 0.82 1.10 1.38 1.65 1.93 2.21 2.71
0.49 0.16 0.26 0.37 0.53 0.64 0.79 1.06 1.33 1.59 1.85 2.12 2.60
0.50 0.15 0.25 0.36 0.51 0.61 0.76 1.01 1.27 1.52 1.78 2.04 2.50
0.51 0.15 0.24 0.34 0.49 0.59 0.73 0.98 1.22 1.46 1.71 1.96 2.40
0.52 0.14 0.23 0.33 0.47 0.57 0.70 0.94 1.18 1.41 1.65 1.88 2.31
0.53 0.14 0.22 0.32 0.45 0.54 0.67 0.91 1.13 1.35 1.59 1.81 2.22
0.54 0.13 0.22 0.31 0.44 0.52 0.65 0.87 1.09 1.30 1.53 1.75 2.14
0.55 0.13 0.21 0.29 0.42 0.51 0.63 0.84 1.05 1.26 1.47 1.68 2.06
0.56 0.12 0.20 0.28 0.41 0.49 0.60 0.81 1.02 1.21 1.42 1.62 1.99
0.57 0.12 0.19 0.27 0.39 0.47 0.58 0.78 0.98 1.17 1.37 1.57 1.92
0.58 0.11 0.19 0.27 0.38 0.45 0.56 0.76 0.95 1.13 1.32 1.51 1.85
0.59 0.11 0.18 0.26 0.37 0.44 0.54 0.73 0.91 1.09 1.28 1.46 1.79
0.60 0.11 0.18 0.25 0.35 0.42 0.53 0.71 0.88 1.06 1.24 1.41 1.73
  • Tolerance of ohm/m: ±5%
  • Round wire: range from 0.04mm (0.0016″) to 12mm (0.4724″)
  • Ribbon: range from 0.05mm (0.002″) to 6mm (0.2362″), Max ratio width : thickness = 10:1

CuNi2 NC005 2.0802 Cupronickel Wire Perfect Solution For Stress Corrosion Cracking And Pitting ResistanceCuNi2 NC005 2.0802 Cupronickel Wire Perfect Solution For Stress Corrosion Cracking And Pitting ResistanceCuNi2 NC005 2.0802 Cupronickel Wire Perfect Solution For Stress Corrosion Cracking And Pitting Resistance